Hi,

I have a 40 foot Silverton and have problem with my zincs they seem to be burning out in about 8 weeks. This is the first time I have ever had any problem like this before. People tend to say well you have a bad electrolysis problem. I say well how do you fix it ?? and then the silence.

If anyone has info on the correct way to test and also the correct way the grounding and bonding and A/C ground systems should be connected that would be great. For now my testing has reveled that the battery ground and the bonding system are tied together, is this correct.?????.

PS

I also installed a Galvanic isolator, did not seen to help.

John
 